309S (UNS S30908, 1.4828, SUS309S) is a high-Cr-Ni austenitic stainless steel, designed for excellent high-temperature oxidation resistance.
UNS: S30908|JIS: SUS309S|GB: 06Cr23Ni13|EN: X5CrNi23-12
C: <=0.08|Si: <=1.00|Mn: <=2.00|P: <=0.045|S: <=0.030|Cr: 22.00-24.00|Ni: 12.00-15.00|Fe: Balance
| 309 | 309S | 309H | |
|---|---|---|---|
| 22.0 min.-24.0 max. | 22.0 min.-24.0 max. | 22.0 min.-24.0 max. | |
| 12.0 min.-15.0 max. | 12.0 min.-15.0 max. | 12.0 min.-15.0 max. | |
| 0.20 | 0.08 | 0.04 min.-0.10 max. | |
| 2.00 | 2.00 | 2.00 | |
| 0.045 | 0.045 | 0.045 | |
| 0.030 | 0.030 | 0.030 | |
| 0.75 | 0.75 | 0.75 | |
Key Properties (20℃, Annealed, Horizontal)
Density: 7.98g/cm³|Melting Point: 1400-1450℃|Tensile Strength: >=515N/mm²|0.2% Yield Strength: >=205N/mm²|Elongation: >=40%|Hardness (HB): <=217
Superior high-temperature oxidation resistance (up to 1050℃); good high-temperature creep strength; excellent weldability; suitable for industrial furnaces and high-temp oxidizing environments.
304 vs 309S (Horizontal)
Cr Content: 304 (18.00-20.00%)|309S (22.00-24.00%)|High-Temp Service: 304 (<=870℃)|309S (<=1050℃)|Oxidation Resistance: 304 (Good)|309S (Excellent)
If you have project requirements for stainless steel, we welcome your order. GNEE has a large inventory of popular products for you to choose from. It can be processed into various practical product forms, including plates, coils, tubes, bars, wires, etc. For detailed chemical composition information and free samples, please contact our factory immediately. We offer competitive prices and excellent service.Email: info@gneestainless.com