Chemcial Composition of Grade 310/310S Stainless Steel
The chemical composition of grade 310 and grade 310S stainless steel are summarised in the following table.
Table 1. Chemical composition % of grade 310 and 310S stainless steel
|
|
310 |
310S |
|
0.25 max |
0.08 max |
|
|
2.00 max |
2.00 max |
|
|
1.50 max |
1.50 max |
|
|
0.045 max |
0.045 max |
|
|
0.030 max |
0.030 max |
|
|
24.00 - 26.00 |
24.00 - 26.00 |
|
|
19.00 - 22.00 |
19.00 - 22.00 |
Mechanical Properties of Grade 310/310S Stainless Steel
The mechanical properties of grade 310 and grade 310S stainless steel are summarised in the following table.
Table 2. Mechanical properties of of grade 310/310S stainless steel
|
|
310/ 310S |
|
Grade 0.2 % Proof Stress MPa (min) |
205 |
|
520 |
|
|
40 |
|
|
225 |